Basic Info.
Additional Info.
SKN-2008B air splicer in applicable for doubling winder, rotary traverse winder and two-for-one twister.
Applicable yarns: Most spun yarns and elastic core yarn.
Applicable count number: Ne6--Ne120(Tex100--Tex6.5).
Air pressure: 0.55--0.75Mpa
Major technique parameter
1. Splicing strength: Not less than 80% of original yarn(Depending on composition with the number of shares which twist and meet the requirement of following process)
2. Splicing strength unevenness: Less than 18%
3. Splicing length: 15--25mm
4. Splicing diameter: Less than 1.1--1.3 times of original yarn diameter
5. Splicing speed: 0.5--1.5 second every time(adjustable)
6. Splicing for air splicer: 0.55--0.75Mpa for common yarn.
Product Description
SKN-2008B air splicer in applicable for doubling winder, rotary traverse winder and two-for-one twister.
Applicable yarns: Most spun yarns and elastic core yarn.
Applicable count number: Ne6--Ne120(Tex100--Tex6.5).
Air pressure: 0.55--0.75Mpa
Major technique parameter
1. Splicing strength: Not less than 80% of original yarn(Depending on composition with the number of shares which twist and meet the requirement of following process)
2. Splicing strength unevenness: Less than 18%
3. Splicing length: 15--25mm
4. Splicing diameter: Less than 1.1--1.3 times of original yarn diameter
5. Splicing speed: 0.5--1.5 second every time(adjustable)
6. Splicing for air splicer: 0.55--0.75Mpa for common yarn.